济南beplay全站app安卓制品缩水的成因及解决办法?

来源:http://www.jnhjgs.cn     发布时间:2021-03-08 13:40:11    点击:

beplay全站app安卓制品缩水的成因
Causes of shrinkage of mould products
1.模腔胶料不足,引起收缩
1. The mold cavity is short of rubber, causing shrinkage
A.填充入料不足或加料量不够
A. Insufficient filling or feeding
B.浇口位置不当或浇口不对称
B. Improper gate position or gate asymmetry
C.分流道,浇口不足或太小
C. Diverter, insufficient or too small gate
D.制品壁厚或厚薄不均匀,在厚壁处的背部容易出现缩水
D. The thickness or thickness of the product is uneven, and the back of the thick wall is easy to shrink
2.工艺技术参数调节不当
2. Improper adjustment of technological parameters
A.射胶压力小,射胶速度慢
A. Low injection pressure and slow injection speed
B.射胶时间设置太短
B. The injection time setting is too short
C.保压时间设置太短
C. Pressure holding time setting too short
D.冷却时间设置帮短
D. The cooling time is set to be shorter
3.塑料过热
3. Plastic overheating
A.塑料过热,熔胶筒温度设置太高
A. The plastic is overheated, and the temperature of the melt glue cylinder is set too high
B.beplay全站app安卓温度过高
B. Mold temperature too high
C.beplay全站app安卓有局部过热或制品脱模时过热
C. The mould is overheated locally or when the product is demoulded
D.料温太低或塑化不良,使融料流动不良
D. Too low material temperature or poor plasticization, resulting in poor melt flow
制品缩水的解决方法
Solution to shrinkage of products
1.进行调节校正
1. Adjust and correct
A.增加加料或开大下料口闸板
A. Increase the feeding or open the gate of blanking port
B.限制熔胶全部流入直浇道浇口,不流入其他浇口
B. Limit all melt into the sprue gate, not into other gates
C.增多分流道和增大浇品尺寸
C. Increasing runner and casting size
D.可对工模beplay全站app安卓进行修改或增加注射压力
D. The mold can be modified or the injection pressure can be increased
                                          济南beplay全站app安卓
2.进行调节校正
2. Adjust and correct
A.调节增大射胶压力和射胶速度
A. Adjust and increase the injection pressure and injection speed
B.增加射胶时间设定值
B. Increase the setting value of injection time
C.增加保压时间设定值
C. Increase the set value of holding time
D.增加冷却时间设定值
D. Increase the cooling time setting
3.进行调节校正
3. Adjust and correct
A.降低熔胶筒的温度设定值
A. Reduce the temperature setting value of the glue cartridge
B.降低模温,调节冷却系统进水闸阀
B. Reduce the mold temperature and adjust the inlet gate valve of cooling system
C.检查工模冷却系统或延长冷却时间
C. Check the cooling system of the die or extend the cooling time
D.增加熔胶筒各段加热区温度,检验塑化胶料的程度
D. Increase the temperature of the heating zone of each section of the melt cartridge, and check the degree of plasticizing compound
联系我们 contact

山东济南beplay全站app安卓_铝合金压铸厂-山东宏捷beplay全站app安卓有限公司

电话1:13173017488

电话2:18615459955

传真:0531-88771136

邮箱:hlm369@126.com

地址:山东省济南市大桥镇大王村北跨商务中心后三层白楼

山东济南beplay全站app安卓_铝合金压铸厂-山东宏捷beplay全站app安卓有限公司 手机: 13173017488 咨询热线: 0531-88771136 咨询热线:18615459955    邮箱:hlm369@126.com

公司地址: 山东省济南市大桥镇大王村北跨商务中心后三层白楼